Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

MDPE XP9000 Korea Daelim Basell
--
Pipeline system
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | Korea Daelim Basell/XP9000 |
---|---|---|---|
Vicat Softening Temperature | ASTMD1525 | 122 °C | |
Peak Melting Temperature | ASTMD3418 | 125 °C |
Physical | Test Condition | Test Method | Korea Daelim Basell/XP9000 |
---|---|---|---|
Melt Mass-Flow Rate | 190°C/2.16kg | ASTMD1238 | 0.60 g/10min |
Environmental Stress Cracking Resistance | 模压成型,F50 | ASTMD1693B | >10000 hr |
Mechanical Properties | Test Condition | Test Method | Korea Daelim Basell/XP9000 |
---|---|---|---|
Flexural Modulus | 模压成型 | ASTMD790 | 588 Mpa |
Tensile Strength | 断裂,模压成型 | ASTMD638 | 39.2 Mpa |
Tensile Elongation | 断裂,模压成型 | ASTMD638 | 850 % |
Optical | Test Condition | Test Method | Korea Daelim Basell/XP9000 |
---|---|---|---|
Gloss | 45°,CompressionMolded | ASTMD2457 | 75 |
Impact Properties | Test Condition | Test Method | Korea Daelim Basell/XP9000 |
---|---|---|---|
notched Izod Impact Strength | -30°C,CompressionMolded | ASTMD256 | 98 J/m |