Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA12 3030JLX8 UBE JAPAN
UBESTA
pipeline,Pipe fittings
UV resistance,Plasticized,Easy to process
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | UBE JAPAN/3030JLX8 |
---|---|---|---|
Rockwell hardness | R-Sale | ISO 2039-2 | 60 |
Shore hardness | ShoreD | ISO 868 | 69 |
thermal performance | Test Condition | Test Method | UBE JAPAN/3030JLX8 |
---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 100 °C |
1.8MPa,Unannealed | ISO 75-2/A | 52.0 °C | |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 1.7E-04 cm/cm/°C |
Melting temperature | ISO 3146 | 173 °C |
mechanical properties | Test Condition | Test Method | UBE JAPAN/3030JLX8 |
---|---|---|---|
Bending modulus | ISO 178 | 400 Mpa | |
bending strength | ISO 178 | 20.0 Mpa | |
Tensile strain | Yield | ISO 527-2 | 32 % |
Break | ISO 527-2 | 200 % | |
tensile strength | Yield | ISO 527-2 | 26.0 Mpa |
Electrical performance | Test Condition | Test Method | UBE JAPAN/3030JLX8 |
---|---|---|---|
Volume resistivity | IEC 60093 | 1E+12 ohms·cm |
Physical properties | Test Condition | Test Method | UBE JAPAN/3030JLX8 |
---|---|---|---|
melt mass-flow rate | 235°C/2.16kg | ISO 1133 | 13 g/10min |
Shrinkage rate | MD | ISO 294-4 | 1.0 % |
TD | ISO 294-4 | 1.3 % | |
Water absorption rate | 23°C,24hr | ISO 62 | 0.60 % |