Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM LO-21 KEP KOREA
KEPITAL®
currency
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | KEP KOREA/LO-21 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 95.0 °C |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 1.3E-04 cm/cm/°C |
| Melting temperature | ISO 11357-3 | 165 °C |
| mechanical properties | Test Condition | Test Method | KEP KOREA/LO-21 |
|---|---|---|---|
| Bending modulus | ISO 178 | 2450 Mpa | |
| ASTM D790/ISO 178 | 355000 kg/cm²(MPa)[Lb/in²] | ||
| bending strength | ASTM D790/ISO 178 | 11700 kg/cm²(MPa)[Lb/in²] | |
| ISO 178 | 81.0 Mpa | ||
| Tensile strain | Yield | ISO 527-2 | 10 % |
| Break | ISO 527-2 | 26 % | |
| tensile strength | ISO 527-2 | 60.0 Mpa |
| Electrical performance | Test Condition | Test Method | KEP KOREA/LO-21 |
|---|---|---|---|
| Surface resistivity | IEC 60093 | 1E+16 ohms | |
| Volume resistivity | IEC 60093 | 1E+14 ohms·cm |
| other | Test Condition | Test Method | KEP KOREA/LO-21 |
|---|---|---|---|
| characteristic | 耐磨性能良好 |
| Physical properties | Test Condition | Test Method | KEP KOREA/LO-21 |
|---|---|---|---|
| density | ASTM D792/ISO 1183 | 1.39 | |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 9.5 g/10min |
| Shrinkage rate | MD:3.00mm | Internal Method | 2.0 % |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.20 % |
| flammability | Test Condition | Test Method | KEP KOREA/LO-21 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |