Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | COVESTRO GERMANY/DP.9095AU |
|---|---|---|---|
| tensile strength | 10% Strain, 23°C | DIN 53504 | 6.40 Mpa |
| Tensile storage modulus | 60°C | ISO 6721 | 82.0 Mpa |
| Tensile strain | Break, 23°C | DIN 53504 | 450 % |
| tensile strength | 300% Strain, 23°C | DIN 53504 | 30.0 Mpa |
| Tensile storage modulus | -20°C | ISO 6721 | 790 Mpa |
| 20°C | ISO 6721 | 161 Mpa | |
| tensile strength | Break, 23°C | DIN 53504 | 52.7 Mpa |
| 100% Strain, 23°C | DIN 53504 | 14.8 Mpa | |
| 50% Strain, 23°C | DIN 53504 | 12.0 Mpa | |
| Wear resistance | ISO 4649 | 18.0 mm³ | |
| hardness | Test Condition | Test Method | COVESTRO GERMANY/DP.9095AU |
| Shore hardness | Shore A, 3 sec | ISO 8682 | 94 |
| Shore D, 1 Sec, 23°C | ISO 7619 | 45 | |
| Shore A, 1 Sec, 23°C | ISO 7619 | 94 | |
| Shore D, 15 sec | ISO 8682 | 45 | |
| elastomer | Test Condition | Test Method | COVESTRO GERMANY/DP.9095AU |
| Permanent compression deformation | 23°C, 72 hr | ISO 815 | 30 % |
| 70°C, 24 hr4 | ISO 815 | 43 % | |
| 70°C, 24 hr6 | ISO 815 | 31 % | |
| Resilience | ISO 4662 | 33 % | |
| tear strength | 23°C | ISO 34-1 | 130 kN/m |
| injection | Test Condition | Test Method | COVESTRO GERMANY/DP.9095AU |
| Mold temperature | 20 °C | ||
| drying temperature | < 100 °C | ||
| Processing (melt) temperature | 200 to 220 °C |