PC HF-1023IM K2261 Samsung Cheil South Korea
INFINO®
Electrical field,Electronic field,Daily products
High impact resistance,High mobility, Impact resistance,High liquidity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic Performance | Test Condition | Test Method | Samsung Cheil South Korea/HF-1023IM K2261 |
---|---|---|---|
melt mass-flow rate | 200℃ 5kg | ASTM D-1238 | 25.0 g/10min |
Water absorption rate | 23℃ | ASTM D-570 | 0.35 % |
thermal performance | Test Condition | Test Method | Samsung Cheil South Korea/HF-1023IM K2261 |
---|---|---|---|
Hot deformation temperature | 18.56kgf/cm2 | ASTM D-648 | 125 °C |
UL flame retardant rating | UL 94 | V-2 | |
Vicat softening temperature | 5kg | ASTM D-1525 | 136 °C |
mechanical properties | Test Condition | Test Method | Samsung Cheil South Korea/HF-1023IM K2261 |
---|---|---|---|
Bending modulus | 2.8mm/min | ASTM D-790 | 1960 Mpa |
bending strength | 2.8mm/min | ASTM D-790 | 90 Mpa |
Impact strength of cantilever beam gap | 1/8" | ASTM D-256 | 736 J/m |
Rockwell hardness | ASTM D-785 | 120 | |
tensile strength | 50mm/min | ASTM D-638 | 62 Mpa |
Physical properties | Test Condition | Test Method | Samsung Cheil South Korea/HF-1023IM K2261 |
---|---|---|---|
Shrinkage rate | ASTM D-955 | 0.5-0.7 % |