Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6T C215NK MITSUI CHEM JAPAN
ARLEN™
Electrical applications、Electronic and electrical
Glass fiber reinforced、Flame retardant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | MITSUI CHEM JAPAN/C215NK |
---|---|---|---|
Melting Temperature | 310 °C | ||
Heat Deflection Temperature | ASTM D-648 | 295 °C | |
Flame retardancy | UL 94 | HB | |
Glass Transition Temperature | 85 °C | ||
Coefficient of Linear Thermal Expansion | ASTM D-696 | 3.4(3.5) |
Physical | Test Condition | Test Method | MITSUI CHEM JAPAN/C215NK |
---|---|---|---|
Moisture Absorption | 23℃,24小时在水里(2mmt,100℃) | ASTM D-570 | 0.4(3.8) % |
Modeling Shrinkage | 2mmt | ASTM D-955 | 0.6(0.9) % |
Mechanical Properties | Test Condition | Test Method | MITSUI CHEM JAPAN/C215NK |
---|---|---|---|
Tensile Strength | dry(moist) | ASTM D-638 | 110(90) Mpa |
Rockwell Hardness | ASTM D-785 | 105 M Scale | |
Flexural Modulus | dry(moist) | ASTM D-790 | 6000(4000) Mpa |
IZOD Notch Impact Strength | dry(moist) | ASTM D-256 | 50(55) J/m |
Flexural Strength | dry(moist) | ASTM D-790 | 180(150) Mpa |
Tensile Elongation?(Break) | dry(moist) | ASTM D-638 | 3(3) % |
Other | Test Condition | Test Method | MITSUI CHEM JAPAN/C215NK |
---|---|---|---|
Glass fiber content | 15 % |
Electrical Properties | Test Condition | Test Method | MITSUI CHEM JAPAN/C215NK |
---|---|---|---|
Dielectric Constant | 10 | ASTM D-150 | 4.2 |
Dielectric breakdown voltage | dry | ASTM D-149 | 25 KV/mm |
Loss factor | 10 | ASTM D-150 | 0.020 |
Volume Resistivity | dry | ASTM D-257 | 10 Ω.cm |