Ethylene Copolymer Escorene™ Ultra LD 723.28 Cast ExxonMobil
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Test Condition | Test Method | ExxonMobil/Escorene™ Ultra LD 723.28 Cast | |
---|---|---|---|
Vinyl acetate content | ExxonMobilMethod | 18.5 wt% | |
Secant modulus | 1%正割,TD | ASTM D882 | 55.3 MPa |
elongation | TD:断裂 | ASTM D882 | 810 % |
melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 23 g/10min |
Secant modulus | 1%正割,MD | ASTM D882 | 50.9 MPa |
elongation | MD:断裂 | ASTM D882 | 530 % |
Elmendorf tear strength | MD | ASTM D1922 | 240 g |
Haze ratio | ASTM D1003 | 0.90 % | |
gloss | 45° | ASTM D2457 | 89 |
tensile strength | MD:断裂 | ASTM D882 | 21.6 MPa |
Elmendorf tear strength | TD | ASTM D1922 | 330 g |
Dart impact | ASTM D1709 | 94 g | |
tensile strength | TD:断裂 | ASTM D882 | 14.9 MPa |
vicat | ASTM D1525 | 54.0 °C |