PA6/66 T4381LDS BASF GERMANY
Ultramid®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | BASF GERMANY/T4381LDS |
|---|---|---|---|
| Hot deformation temperature | Unannealed0.45MPa,545MPa | ISO 75 | 265 °C |
| Linear coefficient of thermal expansion | Flow | ISO 11359 | 3E-5 cm/cm/℃ |
| 垂直__ | ISO 11359 | 5E-5 cm/cm/℃ | |
| Melting temperature | ISO 11357 | 295 °C |
| flame retardant performance | Test Condition | Test Method | BASF GERMANY/T4381LDS |
|---|---|---|---|
| UL flame retardant rating | 1.6mm | UL 94 | HB |
| mechanical properties | Test Condition | Test Method | BASF GERMANY/T4381LDS |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | 4 kJ/m² | |
| 23℃ | ISO 179 | 35 kJ/m² | |
| elongation | 23℃ | ISO 527 | 2 % |
| Tensile modulus | 23℃ | ISO 527 | 8300 Mpa |
| tensile strength | 23℃ | ISO 527 | 105 Mpa |
| Electrical performance | Test Condition | Test Method | BASF GERMANY/T4381LDS |
|---|---|---|---|
| Dielectric constant | 1MHz | IEC 60250 | 0.0015 |
| Volume resistivity | IEC 60093 | 1E15 Q.cm |
| Physical properties | Test Condition | Test Method | BASF GERMANY/T4381LDS |
|---|---|---|---|
| density | ISO 1183 | 1.57 g/cm³ | |
| Shrinkage rate | Flow | ISO 294 | 0.55 % |
| 垂直 | ISO 294 | 0.75 % | |
| Water absorption rate | 23°C50RH | ISO 62 | 1 % |
| 23℃ 24hr | ISO 62 | 4.7 % |