Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPA T4 GF 50 black (3661) AKRO-PLASTIC GmbH
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | AKRO-PLASTIC GmbH/ T4 GF 50 black (3661) |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 15 kJ/m² |
-30°C | ISO 179/1eA | 13 kJ/m² | |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 95 kJ/m² |
-30°C | ISO 179/1eU | 90 kJ/m² |
Supplementary Information | Test Condition | Test Method | AKRO-PLASTIC GmbH/ T4 GF 50 black (3661) |
---|---|---|---|
ReinforcementContent | ISO 1172 | 50 % |
Mechanical properties | Test Condition | Test Method | AKRO-PLASTIC GmbH/ T4 GF 50 black (3661) |
---|---|---|---|
tensile strength | 断裂 | ISO 527-2/5 | 280 MPa |
Tensile strain | 断裂 | ISO 527-2/5 | 2.3 % |
Flexural modulus | ISO 178 | 17700 MPa | |
Tensile modulus | ISO 527-2/1 | 18000 MPa | |
bending strength | ISO 178 | 400 MPa |
flammability | Test Condition | Test Method | AKRO-PLASTIC GmbH/ T4 GF 50 black (3661) |
---|---|---|---|
burning rate | 1.00mm | FMVSS302 | <100 mm/min |
UL flame retardant rating | 0.8mm | UL 94 | HB |
physical property | Test Condition | Test Method | AKRO-PLASTIC GmbH/ T4 GF 50 black (3661) |
---|---|---|---|
density | 23°C | ISO 1183 | 1.62 g/cm³ |
Shrinkage rate | TD | ISO 294-4 | 0.70 % |
MD | ISO 294-4 | 0.20 % |
Thermal performance | Test Condition | Test Method | AKRO-PLASTIC GmbH/ T4 GF 50 black (3661) |
---|---|---|---|
melting temperature | DIN EN11357-1 | 295 °C | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 260 °C |