Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

EVA 5-2 BEIJING EASTERN
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Basic Performance | Test Condition | Test Method | BEIJING EASTERN/5-2 |
|---|---|---|---|
| density | ASTM D-1505 | 0.925 | |
| melt mass-flow rate | ASTM D-1238 | 2 g/10 |
| thermal performance | Test Condition | Test Method | BEIJING EASTERN/5-2 |
|---|---|---|---|
| Melting temperature | 104 °C | ||
| 104 ℃(℉) | |||
| Vicat softening temperature | ASTM D-1525 | 90 °C |
| mechanical properties | Test Condition | Test Method | BEIJING EASTERN/5-2 |
|---|---|---|---|
| Elongation at Break | ASTM D-6398 | 620 % | |
| ASTM D638/ISO 527 | 27 % | ||
| Impact strength of cantilever beam gap | ASTM D-1709 A-B | 大于等于140 g | |
| Secant modulus | 1%Strain, Break | ASTM D-882B | 130 N/mm |
| Shore hardness | ASTM D2240/ISO 868 | 40 Shore D | |
| ASTM D-2240 | 40 | ||
| ASTM D2240/ISO 868 | 95 Shore A | ||
| tear strength | ASTM D-1922 | 167 g | |
| tensile strength | Break | ASTM D-638 | 19 N/mm |
| Yield | ASTM D-638 | 7.5 N/mm |
| Electrical performance | Test Condition | Test Method | BEIJING EASTERN/5-2 |
|---|---|---|---|
| Dielectric constant | ASTM D150/IEC 60250 | 750 | |
| ASTM D-150 | 2.6 | ||
| Dielectric strength | ASTM D-149 | 750 KV/cm |
| Physical properties | Test Condition | Test Method | BEIJING EASTERN/5-2 |
|---|---|---|---|
| density | ASTM D1505 | 0.925 g/cm² | |
| film thickness | 40 u | ||
| gloss | ASTM D-1003A | 70 % | |
| turbidity | ASTM D-2457 | 5 % | |
| Vinyl acetate content | ISC.DIS 8965/1989(E) | 5 % | |
| 5 % |