Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU STARLEX E/8025-88 naturale Daloga srl
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Daloga srl/STARLEX E/8025-88 naturale |
|---|---|---|---|
| Shore hardness | ShoreA,30Sec | ISO 868 | 88to92 |
| thermal performance | Test Condition | Test Method | Daloga srl/STARLEX E/8025-88 naturale |
|---|---|---|---|
| Brittle temperature | ISO 458 | -43.0--39.0 °C | |
| thermal stability | ISO R182 | >80 | |
| Usage temperature | ISO 1183 | 90 °C |
| mechanical properties | Test Condition | Test Method | Daloga srl/STARLEX E/8025-88 naturale |
|---|---|---|---|
| Tensile strain | Break | ISO 527-2 | 450to550 % |
| tensile strength | Yield | ISO 527-2 | 28.8to35.2 MPa |
| Wear resistance | DIN 53516 | 47.5to52.5 mm³ |
| Physical properties | Test Condition | Test Method | Daloga srl/STARLEX E/8025-88 naturale |
|---|---|---|---|
| density | ISO 1183 | 1.22to1.26 g/cm³ |
| flammability | Test Condition | Test Method | Daloga srl/STARLEX E/8025-88 naturale |
|---|---|---|---|
| Extreme Oxygen Index | ISO 4589-2 | 26to29 % | |
| UL flame retardant rating | UL 94 | V-0 |
| elastomer | Test Condition | Test Method | Daloga srl/STARLEX E/8025-88 naturale |
|---|---|---|---|
| tear strength | ASTM D624 | 61.8to68.3 kN/m |