Impact resistance | Test Condition | Test Method | DSM HOLAND/TS272A1 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 5.0 kJ/m² |
Mechanical properties | Test Condition | Test Method | DSM HOLAND/TS272A1 |
---|---|---|---|
Tensile modulus | ISO 527-2 | 2800 Mpa | |
Tensile strain | 断裂 | ISO 527-2 | 20 % |
Flexural modulus | ISO 178 | 2400 Mpa | |
tensile strength | 断裂 | ISO 527-2 | 80.0 Mpa |
physical property | Test Condition | Test Method | DSM HOLAND/TS272A1 |
---|---|---|---|
Water absorption rate | 平衡, 23°C, 50% RH | ISO 62 | 3.0 % |
density | ISO 1183 | 1.26 g/cm³ | |
Shrinkage rate | 流量 | ISO 294-4 | 2.2 % |
横向流量 | ISO 294-4 | 2.2 % |
Thermal performance | Test Condition | Test Method | DSM HOLAND/TS272A1 |
---|---|---|---|
melting temperature | ISO 11357-3 | 295 °C | |
Heat distortion temperature | 1.8 MPa, 未退火,HDT | ISO 75-2/A | 160 °C |