Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| squeeze out | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
|---|---|---|---|
| Melt Temperature | 220 to 250 °C | ||
| drying temperature | 70 to 80 °C | ||
| drying time | 5.0 to 7.0 hr | ||
| mechanical properties | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
| Nominal tensile fracture strain | ISO 527-2 | > 50 % | |
| tensile strength | Yield | ISO 527-2 | 23.0 Mpa |
| Tensile modulus | ISO 527-2 | 414 Mpa | |
| Tensile strain | Yield | ISO 527-2 | 22 % |
| Wear resistance | ISO 4649 | 41.0 mm³ | |
| Physical properties | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 1.4 % |
| Shrinkage rate | Flow | ISO 294-4 | 1.2 % |
| 横向Flow | ISO 294-4 | 1.5 % | |
| Water absorption rate | Saturation, 23°C | ISO 62 | 0.76 % |
| injection | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
| Mold temperature | 25 to 60 °C | ||
| drying temperature | 70 to 80 °C | ||
| Processing (melt) temperature | 230 to 290 °C | ||
| drying time | 5.0 to 7.0 hr | ||
| hardness | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
| Shore hardness | Shore D, 15 Sec | ISO 7619-1 | 61 |
| impact performance | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | -- |
| -30°C | ISO 179/1eU | -- | |
| thermal performance | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
| Melting temperature | ISO 11357-3 | 172 °C | |
| Vicat softening temperature | ISO 306/B50 | 129 °C |