Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA12 7033 SA01 MED ARKEMA USA
--
Medical and nursing supplies
Low wear
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
---|---|---|---|
Shore hardness | Shore D, 15 Sec | ISO 7619-1 | 61 |
thermal performance | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
---|---|---|---|
Melting temperature | ISO 11357-3 | 172 °C | |
Vicat softening temperature | ISO 306/B50 | 129 °C |
mechanical properties | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
---|---|---|---|
Nominal tensile fracture strain | ISO 527-2 | > 50 % | |
Tensile modulus | ISO 527-2 | 414 Mpa | |
Tensile strain | Yield | ISO 527-2 | 22 % |
tensile strength | Yield | ISO 527-2 | 23.0 Mpa |
Wear resistance | ISO 4649 | 41.0 mm³ |
Physical properties | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
---|---|---|---|
Shrinkage rate | 横向Flow | ISO 294-4 | 1.5 % |
Flow | ISO 294-4 | 1.2 % | |
Water absorption rate | Saturation, 23°C | ISO 62 | 0.76 % |
Equilibrium, 23°C, 50% RH | ISO 62 | 1.4 % |
impact performance | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
---|---|---|---|
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | -- |
23°C | ISO 179/1eU | -- |
squeeze out | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
---|---|---|---|
drying temperature | 70 to 80 °C | ||
drying time | 5.0 to 7.0 hr | ||
Melt Temperature | 220 to 250 °C |
injection | Test Condition | Test Method | ARKEMA USA/7033 SA01 MED |
---|---|---|---|
drying temperature | 70 to 80 °C | ||
drying time | 5.0 to 7.0 hr | ||
Mold temperature | 25 to 60 °C | ||
Processing (melt) temperature | 230 to 290 °C |