HDPE DMDA-8950 NT 7 DOW USA
DOW™
Thin-walled container
High impact resistance、Easy to process
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | DOW USA/DMDA-8950 NT 7 |
---|---|---|---|
Peak Crystallization Temperature? | DSC | Internal Method | 115 °C |
Brittleness Temperature | ASTM D746 | -52.8 °C | |
Melting Temperature | DSC | Internal Method | 127 °C |
Mechanical Properties | Test Condition | Test Method | DOW USA/DMDA-8950 NT 7 |
---|---|---|---|
Tensile Impact Strength | ASTM D1822 | 90.4 kJ/m² | |
Flexural Modulus | 2% 正割 | ASTM D790B | 576 Mpa |
Tensile Strength | 屈服 | ASTM D638 | 20.9 Mpa |
Tensile Elongation | 9.0 % |
Physical | Test Condition | Test Method | DOW USA/DMDA-8950 NT 7 |
---|---|---|---|
Environmental Stress Cracking Resistance | 50℃, 10% Igepal, F50 | ASTM D1693 | 6.00 hr |
Melt index | 190℃/2.16 kg | ASTM D1238 | 50 g/10 min |