Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Fluoro Si Greene 409 USA Greene
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | USA Greene/Greene 409 |
|---|---|---|---|
| Rockwell hardness | M-Scale | ASTM D785 | 78 |
| Shore hardness | ShoreA | ASTM D2240 | 75 |
| Supplementary Information | Test Condition | Test Method | USA Greene/Greene 409 |
|---|---|---|---|
| RubberClassification | FVMQ | ||
| tear strength | BieB法 | ASTM D624 | 17.5 kN/m |
| TR | ASTM D1329 | -65 °C |
| thermal performance | Test Condition | Test Method | USA Greene/Greene 409 |
|---|---|---|---|
| Linear coefficient of thermal expansion | ASTME228 | 2.1E-04 cm/cm/°C | |
| Usage temperature | -52-81 °C |
| mechanical properties | Test Condition | Test Method | USA Greene/Greene 409 |
|---|---|---|---|
| Friction coefficient | Itself - Static | ASTM D1894 | 1.6 |
| Itself - Dynamic | ASTM D1894 | 0.90 |
| Physical properties | Test Condition | Test Method | USA Greene/Greene 409 |
|---|---|---|---|
| density | ASTM D792 | 1.66 g/cm³ |
| elastomer | Test Condition | Test Method | USA Greene/Greene 409 |
|---|---|---|---|
| elongation | Break | ASTM D1414 | 120 % |
| Permanent compression deformation | 175°C,22hr | ASTM D395 | 15 % |
| tensile strength | 50%Strain | ASTM D1414 | 3.17 MPa |
| 100%Strain | ASTM D1414 | 6.34 MPa | |
| Break | ASTM D1414 | 7.31 MPa |