PP Homopolymer Piolen® P T40A19 PiO Kunststoffe GmbH & Co KG
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodPiO Kunststoffe GmbH & Co KG/Piolen® P T40A19
Charpy Notched Impact Strength23°CISO 179/1eA2.8 kJ/m²
Impact strength of simply supported beam without notch-40°CISO 179/1eU5.7 kJ/m²
23°CISO 179/1eU11 kJ/m²
Charpy Notched Impact Strength-40°CISO 179/1eA1.4 kJ/m²
Mechanical propertiesTest ConditionTest MethodPiO Kunststoffe GmbH & Co KG/Piolen® P T40A19
tensile strength 断裂ISO 527-224.0 MPa
Tensile strain断裂ISO 527-211 %
tensile strength 屈服ISO 527-230.0 MPa
Flexural modulusISO 1783600 MPa
flammabilityTest ConditionTest MethodPiO Kunststoffe GmbH & Co KG/Piolen® P T40A19
UL flame retardant ratingUL 94HB
physical property Test ConditionTest MethodPiO Kunststoffe GmbH & Co KG/Piolen® P T40A19
densityISO 11831.25 g/cm³
melt mass-flow rate230°C/2.16kgISO 113318 g/10min
Thermal performanceTest ConditionTest MethodPiO Kunststoffe GmbH & Co KG/Piolen® P T40A19
Crystallization peak temperatureDSCISO 3146160to170 °C
vicat--ISO 306/B87.0 °C
--ISO 306/A148 °C