Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU-Ester Elastollan® 590 A BASF GERMANY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | BASF GERMANY/Elastollan® 590 A |
---|---|---|---|
Shore hardness | 邵氏D,3秒 | ISO 7619 | 41 |
邵氏A,3秒 | ISO 7619 | 94 |
Mechanical properties | Test Condition | Test Method | BASF GERMANY/Elastollan® 590 A |
---|---|---|---|
Wear amount | ISO 4649-A | 35.0 mm³ |
physical property | Test Condition | Test Method | BASF GERMANY/Elastollan® 590 A |
---|---|---|---|
density | ISO 1183/A | 1.25 g/cm³ |
elastomer | Test Condition | Test Method | BASF GERMANY/Elastollan® 590 A |
---|---|---|---|
tensile strength | 屈服 | DIN 53504 | 50.0 MPa |
tear strength | ISO 34-1 | 100 kN/m | |
elongation | 断裂 | DIN 53504 | 600 % |
Contact Us
Get App
Top