PUR-Capro LFP 2950A CHEMTURU USA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | CHEMTURU USA/ LFP 2950A |
---|---|---|---|
Dynamic Properties | TangentDelta:30°C | 0.0150 | |
StorageModulus:150°C | 2.1E+08 dynes/cm² | ||
TangentDelta:150°C | 0.0130 | ||
StorageModulus:30°C | 3.2E+08 dynes/cm² |
hardness | Test Condition | Test Method | CHEMTURU USA/ LFP 2950A |
---|---|---|---|
Shore hardness | 邵氏A | ASTM D2240 | 94to96 |
Mechanical properties | Test Condition | Test Method | CHEMTURU USA/ LFP 2950A |
---|---|---|---|
compressive strength | 20%应变 | ASTM D695 | 11.7 MPa |
10%应变 | ASTM D695 | 5.52 MPa | |
25%应变 | ASTM D695 | 15.2 MPa | |
5%应变 | ASTM D695 | 2.76 MPa | |
15%应变 | ASTM D695 | 8.27 MPa |
thermosetting | Test Condition | Test Method | CHEMTURU USA/ LFP 2950A |
---|---|---|---|
STORAGE STABILITY | 9.0 min | ||
Post curing time | 127°C | 16 hr | |
stripping time | >60 min |
elastomer | Test Condition | Test Method | CHEMTURU USA/ LFP 2950A |
---|---|---|---|
compression set | 100°C,22hr | ASTM D395B | 60 % |
elongation | 断裂 | ASTM D412 | 580 % |
tear strength | 开裂 | ASTM D470 | 25 kN/m |
Shore hardness | ASTM D2632 | 62 % | |
compression set | 70°C,22hr | ASTM D395B | 45 % |
tensile strength | ASTM D412 | 44.8 MPa | |
300%应变 | ASTM D412 | 13.8 MPa | |
100%应变 | ASTM D412 | 10.3 MPa |
physical property | Test Condition | Test Method | CHEMTURU USA/ LFP 2950A |
---|---|---|---|
density | ASTM D792 | 1.15 g/cm³ |