Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
LCP A430 JAPAN POLYPLASTIC
LAPEROS® 
Electrical applications、Home appliance components
Electrical performance、wear resistant、Lubricity、Halogen-free、Flame retardant、Good electrical performan、Flame retardant、lubrication、Good wear resistance
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Basic performanceTest ConditionTest MethodJAPAN POLYPLASTIC/A430
densityISO 11831500 kg/m
Mechanical propertiesTest ConditionTest MethodJAPAN POLYPLASTIC/A430
Impact strength of simply supported beam without notch23℃ISO 179/1eU86.0 KJ/m
Suspended wall beam without notch impact strength23℃ISO 180/1U67.0 KJ/m
Impact strength of cantilever beam gap23℃ISO 180/1A35.0 KJ/m
Flexural modulus23℃ISO 1787000 Mpa
Charpy Notched Impact Strength23℃ISO 179/1eA28.0 KJ/m
Tensile modulusISO 527-17000 Mpa
Rockwell hardnessISO 2039-255 M Scale
tensile strength ISO 527-1160 Mpa
elongation断裂ISO 527-16.2 %
bending strength23℃ISO 178125 Mpa
Electrical performanceTest ConditionTest MethodJAPAN POLYPLASTIC/A430
relative permittivity1000HzIEC 602502.70
dielectric strengthIEC 60243-136 KV/mm
relative permittivity100HzIEC 602503.30
Volume resistivityIEC 600931E+13 ohm.m
Dielectric loss100HzIEC 602500.030
Compared to the Leakage Traceability Index (CTI)IEC 60112225
Surface ResistivityIEC 600931E+15 ohms
Dielectric loss1000HzIEC 602500.016
physical property Test ConditionTest MethodJAPAN POLYPLASTIC/A430
Shrinkage rateparallelISO 25770.70 %
normalISO 25770.0 %
Thermal performanceTest ConditionTest MethodJAPAN POLYPLASTIC/A430
Heat distortion temperature0.45MPa,HDTISO 75-1227 °C
Linear coefficient of thermal expansionnormalISO 11359-10.000046 cm/cm℃
parallelISO 11359-11E-06 cm/cm℃
combustibilityUL 94V-0
Heat distortion temperature1.80MPa,HDTISO 75-1165 °C
vicat50℃/h 50NISO 306138 °C
Heat distortion temperature8.00MPa,HDTISO 75-189.0 °C

Contact Us

Get App

Top