PBT+ASA TAROLOX 200 G3 Taro Plast S.p.A.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodTaro Plast S.p.A./TAROLOX 200 G3
Charpy Notched Impact Strength23°CISO 179/1eA5.1 kJ/m²
Impact strength of cantilever beam gap23°CASTM D25662 J/m
Supplementary InformationTest ConditionTest MethodTaro Plast S.p.A./TAROLOX 200 G3
ReinforcementContent150°CISO 345115 %
Mechanical propertiesTest ConditionTest MethodTaro Plast S.p.A./TAROLOX 200 G3
Flexural modulusISO 1784100 MPa
Tensile strain断裂ISO 527-2/503.0 %
Tensile modulusISO 527-2/15000 MPa
bending strengthISO 178115 MPa
tensile strength 断裂ISO 527-2/5085.0 MPa
Electrical performanceTest ConditionTest MethodTaro Plast S.p.A./TAROLOX 200 G3
Compared to the Leakage Tracking Index (CTI)解决方案AIEC 60112PLC 1
flammabilityTest ConditionTest MethodTaro Plast S.p.A./TAROLOX 200 G3
Burning wire flammability index2.0mmIEC 60695-2-12650 °C
UL flame retardant rating1.6mmUL 94HB
Limiting Oxygen IndexASTM D286320 %
physical property Test ConditionTest MethodTaro Plast S.p.A./TAROLOX 200 G3
melt mass-flow rate250°C/2.16kgISO 113310 g/10min
Shrinkage rateMD内部方法0.35to0.60 %
Water absorption rate23°C,24hrISO 620.050 %
饱和,23°CISO 620.25 %
Shrinkage rateTD内部方法0.60to0.90 %
densityISO 11831.33 g/cm³
Thermal performanceTest ConditionTest MethodTaro Plast S.p.A./TAROLOX 200 G3
melting temperatureISO 11357-3220 °C
vicatISO 306/B50175 °C
Heat distortion temperature1.8MPa,未退火,HDTISO 75-2/A165 °C