Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | CELANESE USA/7130 NC010 |
|---|---|---|---|
| Tensile modulus | ISO 527-2/1A/1 | 17000 Mpa | |
| tensile strength | Break | ISO 527-2/1A/5 | 150 Mpa |
| Bending modulus | 23°C | ISO 178 | 13000 Mpa |
| bending strength | 23°C | ISO 178 | 210 Mpa |
| Tensile strain | Break | ISO 527-2/1A/5 | 1.5 % |
| flammability | Test Condition | Test Method | CELANESE USA/7130 NC010 |
| UL flame retardant rating | 0.40mm | UL 94 | V-0 |
| Extreme Oxygen Index | ISO 4589-2 | 45 % | |
| Electrical performance | Test Condition | Test Method | CELANESE USA/7130 NC010 |
| Volume resistivity | IEC 60093 | >1.0E+15 ohms·cm | |
| Dissipation factor | 1MHz | IEC 60250 | 0.030 |
| Relative permittivity | 100Hz | IEC 60250 | 4.10 |
| Surface resistivity | IEC 60093 | >1.0E+15 ohms | |
| Dissipation factor | 100Hz | IEC 60250 | 0.014 |
| Relative permittivity | 1MHz | IEC 60250 | 3.70 |
| Dielectric strength | IEC 60243-1 | 45 KV/mm | |
| thermal performance | Test Condition | Test Method | CELANESE USA/7130 NC010 |
| Glass transition temperature | ISO 11357-2 | 120 °C | |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 6.2E-05 cm/cm/°C |
| MD | ISO 11359-2 | 3E-06 cm/cm/°C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 310 °C |
| Melting temperature | ISO 11357-3 | 352 °C | |
| Physical properties | Test Condition | Test Method | CELANESE USA/7130 NC010 |
| Shrinkage rate | MD | ISO 294-4 | 0.010 % |
| TD | ISO 294-4 | 0.60 % | |
| impact performance | Test Condition | Test Method | CELANESE USA/7130 NC010 |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 30 kJ/m² |
| Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 30 kJ/m² |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 22 kJ/m² |