PPS PPS-hGR30 SICHUAN DEYANG
--
Aerospace,Mechanical components,Electrical appliances,Electronic field,Electrical field
enhance
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic Performance | Test Condition | Test Method | SICHUAN DEYANG/PPS-hGR30 |
---|---|---|---|
density | GB/T 1033-1986 | 1.55 g/cm³ |
thermal performance | Test Condition | Test Method | SICHUAN DEYANG/PPS-hGR30 |
---|---|---|---|
Combustibility | 垂直法 | GB/T 2408-1996 | FV-0 级 |
Hot deformation temperature | 1.80MPa | GB/T 1634-1979(1989) | 267 °C |
Melting temperature | GB/T 4608-1984 | 282 °C | |
282 ℃(℉) |
mechanical properties | Test Condition | Test Method | SICHUAN DEYANG/PPS-hGR30 |
---|---|---|---|
Bending modulus | GB/T 1042-1992 | 1.1×104 Mpa | |
ASTM D790/ISO 178 | 1.1*100000 kg/cm²(MPa)[Lb/in²] | ||
bending strength | ASTM D790/ISO 178 | 180 kg/cm²(MPa)[Lb/in²] | |
GB/T 1042-1992 | 180 Mpa | ||
compressive strength | GB/T 1041-1992 | 140 Mpa | |
elongation | Break | GB/T 1040-1992 | 1.70 % |
Elongation at Break | ASTM D638/ISO 527 | 1.7 % | |
Impact strength of cantilever beam gap | GB/T 1843-1996 | 11.5 kJ/m² | |
Rockwell hardness | ASTM D785 | 100 | |
GB/T 9342-1988 | 100 hr | ||
tensile strength | ASTM D638/ISO 527 | 142 kg/cm²(MPa)[Lb/in²] | |
GB/T 1040-1992 | 142 Mpa |
Electrical performance | Test Condition | Test Method | SICHUAN DEYANG/PPS-hGR30 |
---|---|---|---|
Dielectric constant | 1MHz | GB/T 1409-1988 | 4 |
Dielectric strength | GB/T 1408.1-1999 | 18.56 KV/mm | |
Surface resistivity | GB/T 1410-1989 | 2.3×1015 Ω | |
Volume resistivity | GB/T 1410-1989 | 1.0×1015 Ω.m |
Physical properties | Test Condition | Test Method | SICHUAN DEYANG/PPS-hGR30 |
---|---|---|---|
density | ASTM D792/ISO 1183 | 1.55 | |
Shrinkage rate | GB/T 15585-1995 | 0.0025 mm/mm |