| Physical properties | Test Condition | Test Method | BASF GERMANY/8333G |
|---|---|---|---|
| Water absorption rate | (23°C,50RH) | ISO 62 | 1.50 % |
| (23°C,24hr) | ISO 62 | 0.90 % | |
| Electrical performance | Test Condition | Test Method | BASF GERMANY/8333G |
| Dissipation factor | 23°C | IEC 60250 | 0.010 100HZ |
| Dielectric constant | 23°C | IEC 60250 | 3.40 100HZ |
| Volume resistivity | IEC 60093 | 1E+10 Ω.cm | |
| Dissipation factor | 相对漏电起痕指数 | IEC 60112 | 600 V |
| Dielectric strength | IEC 60243-1 | 11 KV/mm | |
| mechanical properties | Test Condition | Test Method | BASF GERMANY/8333G |
| Tensile modulus | -40°C | ISO 527-2 | 9200 Mpa |
| Bending modulus | 23°C | ISO 178 | 7200 Mpa |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 21 kJ/m² |
| tensile strength | 23°C | ISO 527-2 | 145 Mpa |
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 10 kJ/m² |
| bending strength | 23°C | ISO 178 | 215 Mpa |
| Elongation at Break | 23°C | ISO 527-2 | 3.5 % |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 78 kJ/m² |
| Tensile modulus | 23°C | ISO 527-2 | 9300 Mpa |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 20 kJ/m² |
| Impact strength of cantilever beam gap | -40°C | ISO 180/1A | 14 kJ/m² |
| flame retardant performance | Test Condition | Test Method | BASF GERMANY/8333G |
| Ignition temperature of heating wire | 3.00mm | IEC 60695-2-12 | 750 °C |
| Relative temperature of heating wire | 3.00mm | IEC 60695-2-13 | 960 °C |
| UL flame retardant rating | UL -94 | HB 0.80mm | |
| thermal performance | Test Condition | Test Method | BASF GERMANY/8333G |
| Vicat softening temperature | Melting Temperature | ISO 11357-3 | 220 °C |
| Hot deformation temperature | 1.80MPaAnnealed | ISO 75-2/Af | 205 °C |
| 0.45MPaUnannealed | ISO 75-2/Bf | 220 °C |