Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 PFD04ES-BKNAT SABIC INNOVATIVE US
LNP™ STAT-KON™
Fitness equipment,Plastic bag,Electronic and Electrical Applications
Thermal stability,Glass fiber reinforced,Antistatic,Filler: Glass charcoal po
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/PFD04ES-BKNAT |
---|---|---|---|
0.45MPa, unannealed, 64.0mm span | ISO 75-2/Bf | 214 °C | |
1.8MPa, unannealed, 64.0mm span of | ISO 75-2/Af | 195 °C | |
Linear coefficient of thermal expansion | MD:23to60°C | ISO 11359-2 | 3.5E-05 cm/cm/°C |
TD:23to60°C | ISO 11359-2 | 1.1E-04 cm/cm/°C |
mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/PFD04ES-BKNAT |
---|---|---|---|
Bending modulus | ISO 178 | 5900 Mpa | |
bending strength | ISO 178 | 152 Mpa | |
Tensile modulus | ISO 527-2/1 | 7000 Mpa | |
Tensile strain | Break | ISO 527-2/5 | 2.6 % |
tensile strength | Yield | ISO 527-2/5 | 107 Mpa |
Electrical performance | Test Condition | Test Method | SABIC INNOVATIVE US/PFD04ES-BKNAT |
---|---|---|---|
Surface resistivity | ASTM D257 | 1.0E+4-1.0E+6 ohms |
Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/PFD04ES-BKNAT |
---|---|---|---|
Shrinkage rate | MD | Internal Method | 0.40-0.60 % |
Water absorption rate | 23°C,24hr | ISO 62 | 1.0 % |
impact performance | Test Condition | Test Method | SABIC INNOVATIVE US/PFD04ES-BKNAT |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 11 kJ/m² |
Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 50 kJ/m² |