Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA12 LKN-5H EMS-CHEMIE SWITZERLAND
Grilamid® 
Fitness equipment、Electronic and electrical
High temperature resistan、High impact resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodEMS-CHEMIE SWITZERLAND/LKN-5H
Charpy Notched Impact Strength23℃23°CISO 179/1eA5 kJ/m²
-30℃-30°CISO 179/1eA4 kJ/m²
Impact strength of simply supported beam without notch-30℃-30°CISO 179/1eU-- kJ/m²
23℃23°CISO 179/1eU130 kJ/m²
Electrical performanceTest ConditionTest MethodEMS-CHEMIE SWITZERLAND/LKN-5H
dielectric strengthIEC 60243-1-- KV/mm
Volume resistivityIEC 60093-- ohms·cm
Surface ResistivityIEC 60093-- ohms
Compared to the Leakage Tracking Index (CTI)IEC 60112 V
Mechanical propertiesTest ConditionTest MethodEMS-CHEMIE SWITZERLAND/LKN-5H
Tensile strain屈服屈服ISO 527-25 %
Tensile modulusISO 527-22600 Mpa
Shore hardness邵氏 D,15 秒邵氏 D,15 秒ISO 868--
Nominal tensile fracture strainISO 527-220 %
tensile strength 屈服YieldISO 527-250 Mpa
断裂BreakISO 527-250 Mpa
Flame retardant performanceTest ConditionTest MethodEMS-CHEMIE SWITZERLAND/LKN-5H
Flammability levelUL 94HB
physical property Test ConditionTest MethodEMS-CHEMIE SWITZERLAND/LKN-5H
Shrinkage rateMDFlowISO 294-40.8 %
Water absorption rate平衡,23℃,50% RHEquilibrium, 73°F, 50% RHISO 620.4 %
饱和,23℃Saturation, 73°FISO 620.8 %
densityISO 11831.44 g/cm³
Shrinkage rateTDAcross FlowISO 294-40.9 %
Thermal performanceTest ConditionTest MethodEMS-CHEMIE SWITZERLAND/LKN-5H
melting temperatureISO 11357-3178 °C
Heat distortion temperature1.8 MPa,未退火264 psi, Unannealed,HDTISO 75-2/A65 °C
8.0 MPa,未退火1160 psi, Unannealed,HDTISO 75-2/C40 °C
Linear coefficient of thermal expansionTDTransverseISO 11359-20.00012 1/℃
Continuous use temperature---- 44内部方法150 °C
---- 33ISO 257890.0 to 120 °C
Linear coefficient of thermal expansionMD流动ISO 11359-20.00012 1/℃

Contact Us