Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPEE PELPRENE™ P40H TOYOBO CO., LTD.
--
currency
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | TOYOBO CO., LTD./PELPRENE™ P40H |
---|---|---|---|
Impact strength of cantilever beam gap | ASTM D256 | 无断裂 |
hardness | Test Condition | Test Method | TOYOBO CO., LTD./PELPRENE™ P40H |
---|---|---|---|
Shore hardness | 邵氏D | ASTM D2240 | 38 |
Mechanical properties | Test Condition | Test Method | TOYOBO CO., LTD./PELPRENE™ P40H |
---|---|---|---|
Taber abraser | 1000Cycles | ASTM D1044 | 20.0 mg |
elongation | 断裂 | ASTM D638 | 690 % |
Flexural modulus | ASTM D790 | 51.0 MPa | |
Compression Modulus | ASTM D695 | 4.50 MPa | |
tensile strength | 屈服 | ASTM D638 | 21.0 MPa |
Electrical performance | Test Condition | Test Method | TOYOBO CO., LTD./PELPRENE™ P40H |
---|---|---|---|
Volume resistivity | ASTM D257 | 2E+12 ohms·cm | |
dielectric strength | ASTM D149 | 20 kV/mm |
flammability | Test Condition | Test Method | TOYOBO CO., LTD./PELPRENE™ P40H |
---|---|---|---|
UL flame retardant rating | UL 94 | HB |
physical property | Test Condition | Test Method | TOYOBO CO., LTD./PELPRENE™ P40H |
---|---|---|---|
Water absorption rate | 平衡,23°C,65%RH | ASTM D570 | 0.48 % |
Shrinkage rate | MD:2.00mm | ASTM D955 | 0.50 % |
density | ASTM D792 | 1.12 g/cm³ | |
melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 10 g/10min |
elastomer | Test Condition | Test Method | TOYOBO CO., LTD./PELPRENE™ P40H |
---|---|---|---|
tensile strength | 50%应变 | ASTM D412 | 6.40 MPa |
compression set | ASTM D395 | 50 % | |
tear strength | ASTM D624 | 98.0 kN/m |
Thermal performance | Test Condition | Test Method | TOYOBO CO., LTD./PELPRENE™ P40H |
---|---|---|---|
vicat | ASTM D1525 | 120 °C | |
brittle temperature | ASTM D746 | -65.0 °C | |
Linear coefficient of thermal expansion | MD | ASTM D696 | 1.7E-04 cm/cm/°C |
melting temperature | DSC | 172 °C |