Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66 A3WG8(BK) BASF GERMANY
Ultramid®
Industrial machinery,Electrical applications
High mobility,Oil resistant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | BASF GERMANY/A3WG8(BK) |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 260 °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 250 °C | |
| Melting temperature | ISO 3146 | 260 °C |
| mechanical properties | Test Condition | Test Method | BASF GERMANY/A3WG8(BK) |
|---|---|---|---|
| Bending modulus | 23°C | ISO 178 | 12000 Mpa |
| Tensile modulus | 23°C | ISO 527-2 | 13200 Mpa |
| Tensile strain | Break,23°C | ISO 527-2 | 3.0 % |
| tensile strength | Break,23°C | ISO 527-2 | 220 Mpa |
| Physical properties | Test Condition | Test Method | BASF GERMANY/A3WG8(BK) |
|---|---|---|---|
| density | ISO 1183 | 1.46 g/cm³ | |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 1.5 % |
| impact performance | Test Condition | Test Method | BASF GERMANY/A3WG8(BK) |
|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179 | 11 kJ/m² |
| 23°C | ISO 179 | 13 kJ/m² | |
| Impact strength of cantilever beam gap | -40°C | ISO 180 | 12 kJ/m² |
| 23°C | ISO 180 | 14 kJ/m² | |
| Impact strength of simply supported beam without notch | -30°C | ISO 179 | 83 kJ/m² |
| 23°C | ISO 179 | 95 kJ/m² |