PPS FZ-8600 BK DIC JAPAN
DIC.PPS
--
Filler: Glass mineral
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | DIC JAPAN/FZ-8600 BK |
---|---|---|---|
Rockwell hardness | ASTM D785 | 100 M(Scale) | |
ASTM D785 | 120 R |
thermal performance | Test Condition | Test Method | DIC JAPAN/FZ-8600 BK |
---|---|---|---|
Hot deformation temperature | 1.80MPaUnannealed | ASTM D648 | 260 °C |
Linear coefficient of thermal expansion | TD | ASTM D696 | 1.8E-05 cm/cm/°C |
MD | ASTM D696 | 1.8E-05 cm/cm/°C |
mechanical properties | Test Condition | Test Method | DIC JAPAN/FZ-8600 BK |
---|---|---|---|
Bending modulus | 23°C | ASTM D790 | 12000 Mpa |
bending strength | 23°C | ASTM D790 | 140 Mpa |
Elongation at Break | 23°C | ASTM D638 | 1.1 % |
Friction coefficient | 静态 | ASTM D3702 | 0.35 |
动态 | ASTM D3702 | 0.35 | |
Impact strength of cantilever beam gap | 23°C | ASTM D256 | 50 J/m |
Tensile modulus | 23°C | ASTM D638 | 12500 Mpa |
泊松比 | 7.58 0.33 | ||
tensile strength | 23°C | ASTM D638 | 100 Mpa |
flame retardant performance | Test Condition | Test Method | DIC JAPAN/FZ-8600 BK |
---|---|---|---|
UL flame retardant rating | UL -94 | V-0 0.800mm |
Electrical performance | Test Condition | Test Method | DIC JAPAN/FZ-8600 BK |
---|---|---|---|
Dielectric constant | 23°C | ASTM D150 | 5.0 1MHz |
Dielectric strength | 1.60mm | ASTM D149 | 16 KV/mm |
Dissipation factor | 耐电弧性 | ASTM D495 | 160 S |
相对漏电起痕指数 | ASTM D3638 | 190 V | |
23°C | ASTM D150 | 6E-03 1MHz | |
Volume resistivity | ASTM D257 | 1E+16 Ω.cm |
Physical properties | Test Condition | Test Method | DIC JAPAN/FZ-8600 BK |
---|---|---|---|
Shrinkage rate | TD | ASTM D995 | 1.00 % |
MD | ASTM D995 | 0.40 % | |
Water absorption rate | (23°C,24hr) | ASTM D570 | 0.02 % |