TPU U-675AL KIN JOIN TAIWAN
--
Fitness equipment、Bottle cap
wear resistant、High mobility
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | KIN JOIN TAIWAN/U-675AL |
---|---|---|---|
Vicat Softening Temperature | ASTM D1525/ISO R306 | 160 ℃(℉) |
Mechanical Properties | Test Condition | Test Method | KIN JOIN TAIWAN/U-675AL |
---|---|---|---|
Shore Hardness (Shore A) | ASTM D2240/ISO 868 | 75 Shore A | |
100% Secant | ASTM D412/ISO 527 | 35 Mpa/Psi | |
300% Secant | 64 Mpa/Psi | ||
Tearing Strength | ASTM D624/ISO 34 | 86 n/mm² | |
Tensile Strength | ASTM D412/ISO 527 | 270 Mpa/Psi |
Other | Test Condition | Test Method | KIN JOIN TAIWAN/U-675AL |
---|---|---|---|
Color | 透明 |
Physical Properties | Test Condition | Test Method | KIN JOIN TAIWAN/U-675AL |
---|---|---|---|
Density | ASTM D792/ISO 2781/JIS K7311 | 1.2 |
Processing | Test Condition | Test Method | KIN JOIN TAIWAN/U-675AL |
---|---|---|---|
Drying conditions | 90.C 3一4小时 | ||
Processing temperature | 185 °C | ||
Mold Temperature | 15一30 °C | ||
Pressure | 60 Mpa |