Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Polyester, TS Haysite Plastics H208 Haysite Reinforced Plastics
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Haysite Reinforced Plastics/Haysite Plastics H208 |
|---|---|---|---|
| Babbitt hardness | ASTM D2583 | 35to40 |
| Supplementary Information | Test Condition | Test Method | Haysite Reinforced Plastics/Haysite Plastics H208 |
|---|---|---|---|
| Temperature rating | 155 °C |
| thermal performance | Test Condition | Test Method | Haysite Reinforced Plastics/Haysite Plastics H208 |
|---|---|---|---|
| thermal conductivity | ASTME1925 | 0.72 W/m/K |
| Electrical performance | Test Condition | Test Method | Haysite Reinforced Plastics/Haysite Plastics H208 |
|---|---|---|---|
| Volume resistivity | ASTM D257 | >1.0E+6 ohms·cm |
| Physical properties | Test Condition | Test Method | Haysite Reinforced Plastics/Haysite Plastics H208 |
|---|---|---|---|
| density | ASTMD792 | 3.27 g/cm³ |