PA66 RS3061HSL BK039A DuPont, European Union
Zytel®
electrical equipment、Fitness equipment
High temperature resistan、Glass fiber reinforced
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | DuPont, European Union/RS3061HSL BK039A |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO179/1eU | 34 kJ/m² |
Mechanical properties | Test Condition | Test Method | DuPont, European Union/RS3061HSL BK039A |
---|---|---|---|
Tensile stress | 屈服 | ISO527-2 | 68.0 Mpa |
Tensile strain | 屈服 | ISO527-2 | 4.5 % |
Tensile modulus | ISO527-2 | 2400 Mpa |
flammability | Test Condition | Test Method | DuPont, European Union/RS3061HSL BK039A |
---|---|---|---|
FMVSS flammability | FMVSS302 | B | |
Burning rate 3 | 1.00mm | ISO3795 | <100 mm/min |
physical property | Test Condition | Test Method | DuPont, European Union/RS3061HSL BK039A |
---|---|---|---|
Shrinkage rate | TD | ISO294-4 | 1.2 % |
Water absorption rate | 饱和,23°C,2.00mm | ISO62 | 3.8 % |
Shrinkage rate | MD | ISO294-4 | 1.2 % |
Water absorption rate | 平衡,23°C,2.00mm,50%RH | ISO62 | 1.7 % |
Thermal performance | Test Condition | Test Method | DuPont, European Union/RS3061HSL BK039A |
---|---|---|---|
Heat Deflection Temperature | 0.45MPa,未退火 | ISO75-2/B | 140 °C |
1.8MPa,未退火 | ISO75-2/A | 50.0 °C | |
Glass transition temperature 2 | ISO11357-2 | 60.0 °C | |
melting temperature | ISO11357-3 | 223 °C |