Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA66 Tislamid® PA66 PA66 30 GFR Tisan
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodTisan/Tislamid® PA66 PA66 30 GFR
Impact strength of cantilever beam gap23°CISO 180/A14 kJ/m²
hardnessTest ConditionTest MethodTisan/Tislamid® PA66 PA66 30 GFR
Shore hardness邵氏DISO 86884
Electrical performanceTest ConditionTest MethodTisan/Tislamid® PA66 PA66 30 GFR
Compared to the Leakage Tracking Index (CTI)3.00mmIEC 60112PLC 1
Mechanical propertiesTest ConditionTest MethodTisan/Tislamid® PA66 PA66 30 GFR
tensile strength 断裂ISO 527-2180 MPa
Tensile strain断裂ISO 527-23.0 %
屈服ISO 527-23.0 %
tensile strength 屈服ISO 527-2180 MPa
flammabilityTest ConditionTest MethodTisan/Tislamid® PA66 PA66 30 GFR
Burning wire flammability index3.0mmIEC 60695-2-12650 °C
UL flame retardant rating1.6mmUL 94HB
physical property Test ConditionTest MethodTisan/Tislamid® PA66 PA66 30 GFR
Shrinkage rate0.30 %
ash contentISO 345130 %
Water absorption rate平衡,23°C,50%RHISO 621.9 %
densityISO 11831.36 g/cm³
Thermal performanceTest ConditionTest MethodTisan/Tislamid® PA66 PA66 30 GFR
vicatISO 306/B120255 °C
melting temperature260to265 °C
Heat distortion temperature0.45MPa,未退火,HDTISO 75-2/Be260 °C

Contact Us