TPU A85P4441 HUNTSMAN GERMANY
IROGRAN®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | HUNTSMAN GERMANY/A85P4441 |
---|---|---|---|
Shore hardness | ShoreA,Injection | ASTM D2240 | 87 |
ShoreA,Injection | ISO 868 | 87 | |
ShoreD,Injection | ISO 868 | 38 | |
ShoreD,Injection | ASTM D2240 | 38 |
thermal performance | Test Condition | Test Method | HUNTSMAN GERMANY/A85P4441 |
---|---|---|---|
TMA | High:635.0μm | Internal Method | 175 °C |
Low:635.0μm | Internal Method | 155 °C |
mechanical properties | Test Condition | Test Method | HUNTSMAN GERMANY/A85P4441 |
---|---|---|---|
Wear resistance | ISO 4649 | 35 mm³ |
Physical properties | Test Condition | Test Method | HUNTSMAN GERMANY/A85P4441 |
---|---|---|---|
Melt Volume Flow Rate (MVR) | 190°C/21.6kg | 65.0 cm3/10min | |
Shrinkage rate | MD:Injection | ASTM D955 | 0.80 % |
elastomer | Test Condition | Test Method | HUNTSMAN GERMANY/A85P4441 |
---|---|---|---|
elongation | Break | ASTM D412 | 550 % |
Break | DIN 53504 | 650 % | |
Permanent compression deformation | 23°C,24hr | ASTM D395 | 25 % |
70°C,24hr | ISO 815 | 45 % | |
70°C,24hr | ASTM D395 | 45 % | |
23°C,24hr | ISO 815 | 25 % | |
tear strength | ISO 34-1 | 60 kN/m | |
ASTM D624 | 98.1 kN/m | ||
tensile strength | 300%Strain | DIN 53504 | 11.0 Mpa |
300%Strain | ASTM D412 | 12.4 Mpa | |
Break | ASTM D412 | 30.3 Mpa | |
Break | DIN 53504 | 40.0 Mpa | |
100%Strain | ASTM D412 | 8.27 Mpa | |
100%Strain | DIN 53504 | 7.00 Mpa |