Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM GB-25 BK JAPAN POLYPLASTIC
DURACON®
Bottle cap,Electronic and electrical components
Glass bead reinforcement,Low warpage,Filler: Glass beads,25% filler by weight,25% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | JAPAN POLYPLASTIC/GB-25 BK |
---|---|---|---|
ColourNumber | CF3500/CD3501 |
thermal performance | Test Condition | Test Method | JAPAN POLYPLASTIC/GB-25 BK |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 110 °C |
Linear coefficient of thermal expansion | MD:23to55°C | Internal Method | 9E-05 cm/cm/°C |
TD:23to55°C | Internal Method | 9E-05 cm/cm/°C |
mechanical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/GB-25 BK |
---|---|---|---|
Bending modulus | ISO 178 | 3800 Mpa | |
bending strength | ISO 178 | 104 Mpa | |
Friction coefficient | Dynamic2 | JISK7218 | 0.37 |
Steel - Dynamic3 | JISK7218 | 0.51 | |
Tensile modulus | ISO 527-2 | 4000 Mpa | |
Tensile strain | Break | ISO 527-2 | 10 % |
tensile strength | ISO 527-2 | 59.0 Mpa | |
Wear factor | 0.060MPa,0.15m/sec4 | JISK7218 | 40 10^-8mm³/N·m |
0.49MPa,0.30m/sec5 | JISK7218 | 500 10^-8mm³/N·m | |
0.060MPa,0.15m/sec7 | JISK7218 | 8000 10^-8mm³/N·m | |
0.49MPa,0.30m/sec6 | JISK7218 | 7000 10^-8mm³/N·m |
Electrical performance | Test Condition | Test Method | JAPAN POLYPLASTIC/GB-25 BK |
---|---|---|---|
Dielectric strength | 3.00mm | IEC 60243-1 | 21 KV/mm |
Physical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/GB-25 BK |
---|---|---|---|
density | ISO 1183 | 1.59 g/cm³ | |
melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 7.0 g/10min |
Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 5.00 cm3/10min |
Shrinkage rate | TD:2.00mm | ISO 294-4 | 1.4 % |
MD:2.00mm | ISO 294-4 | 1.7 % |
impact performance | Test Condition | Test Method | JAPAN POLYPLASTIC/GB-25 BK |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 3.4 kJ/m² |
flammability | Test Condition | Test Method | JAPAN POLYPLASTIC/GB-25 BK |
---|---|---|---|
UL flame retardant rating | UL 94 | HB |