Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU C85A10 BASF GERMANY
Elastollan®
Automotive sector
high strength
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | BASF GERMANY/C85A10 |
---|---|---|---|
Shore hardness | 邵氏A | ASTM D2240 | 85 |
thermal performance | Test Condition | Test Method | BASF GERMANY/C85A10 |
---|---|---|---|
Glass Transition Temperature | 内部方法 | -40.0 °C | |
vicat | ASTM D1525 | 110 °C | |
内部方法 | 100 °C |
mechanical properties | Test Condition | Test Method | BASF GERMANY/C85A10 |
---|---|---|---|
flexural modulus | 注塑 | ASTM D790 | 24.8 Mpa |
Taber abraser | ASTM D1044 | 25.0 mg | |
Tensile modulus | 注塑 | ASTM D412 | 20.7 Mpa |
wear resistance | DIN 53516 | 25 mm³ |
Physical properties | Test Condition | Test Method | BASF GERMANY/C85A10 |
---|---|---|---|
density | ASTM D792 | 1.19 g/cm³ | |
melt mass-flow rate | 200°C/21.6kg | ASTM D1238 | 20to60 g/10min |
flammability | Test Condition | Test Method | BASF GERMANY/C85A10 |
---|---|---|---|
UL flame retardant rating | 3.0mm | UL 94 | HB |
0.9mm | UL 94 | HB |
elastomer | Test Condition | Test Method | BASF GERMANY/C85A10 |
---|---|---|---|
compression set | 70°C,22hr | ASTM D395B | 35 % |
23°C,22hr | ASTM D395B | 25 % | |
elongation | 断裂 | ASTM D412 | 590 % |
tear strength | ASTM D624 | 109 kN/m | |
tensile strength | 300%应变 | ASTM D412 | 15.2 Mpa |
100%应变 | ASTM D412 | 6.89 Mpa | |
ASTM D412 | 41.4 Mpa |