Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
Polyester Alloy Vipel® K190-BHC-26 AOC, L.L.C.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Supplementary InformationTest ConditionTest MethodAOC, L.L.C./Vipel® K190-BHC-26
PeakExotherm197 °C
THIXOTROPIC INDEX2.50
GeltoPeak13.0 min
hardnessTest ConditionTest MethodAOC, L.L.C./Vipel® K190-BHC-26
Barcol HardnessASTM D258345
Mechanical propertiesTest ConditionTest MethodAOC, L.L.C./Vipel® K190-BHC-26
elongation断裂ASTM D6382.4 %
tensile strength ASTM D63858.6 MPa
Tensile modulusASTM D6383400 MPa
Flexural modulusASTM D7903790 MPa
bending strengthASTM D790110 MPa
Uncured PropertiesTest ConditionTest MethodAOC, L.L.C./Vipel® K190-BHC-26
GelTime25°C25 min
Viscosity25°C,BrookfieldLV0.35 Pa·s
density1.14 g/cm³
flammabilityTest ConditionTest MethodAOC, L.L.C./Vipel® K190-BHC-26
fire propagation indexASTME8435.0
Smoke productionASTME84445
physical property Test ConditionTest MethodAOC, L.L.C./Vipel® K190-BHC-26
StyreneContent43 %
Thermal performanceTest ConditionTest MethodAOC, L.L.C./Vipel® K190-BHC-26
Heat distortion temperature1.8MPa,未退火,HDTASTM D648138 °C