Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPE TC8AAZ-S340 KRAIBURG TPE GERMANY
THERMOLAST® K
Phone case,chip,Automotive interior parts,Parts under the hood of a car
Good UV resistance,Good adhesion,Good liquidity,Good weather resistance p
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| mechanical properties | Test Condition | Test Method | KRAIBURG TPE GERMANY/TC8AAZ-S340 |
|---|---|---|---|
| Permanent compression deformation | 23℃,72hr | ISO 815 | 40 % |
| 70℃,24hr | ISO 815 | 80 % | |
| 100℃,24hr | ISO 815 | 60 % | |
| Shore hardness | shore A | ISO 868 | 85 |
| tear strength | ISO 34-1 | 33 kN/m | |
| Tensile strain | Break | ISO 527-2 | 650 % |
| Tensile stress | Yield | ISO 527-2 | 11 Mpa |