Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC GN-3430 TEIJIN JAPAN
PANLITE®
Industrial applications、Camera applications、Electrical components
Flame retardant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | TEIJIN JAPAN/GN-3430 |
---|---|---|---|
Heat Deflection Temperature | 负荷1.813MPa(18.6kgf/cm | JIS K-7207 | 149 °C |
Temperature Index | 冲击式,厚度1.47mm | UL 746B | 120 °C |
Heat Deflection Temperature | 负荷0.451MPa(4.6kgf/cm | JIS K-7207 | 151 °C |
Temperature Index | 电学式,厚度1.47mm | UL 746B | 130 °C |
非冲击式,厚度1.47mm | 130 °C | ||
Coefficient of Linear Thermal Expansion | 流动方向 | ASTM D-696 | 2.0 |
垂直方向 | 5.6 |
Physical | Test Condition | Test Method | TEIJIN JAPAN/GN-3430 |
---|---|---|---|
Moisture Absorption | 24hr,in 23℃ | ASTM D-570 | 0.12 % |
Mechanical Properties | Test Condition | Test Method | TEIJIN JAPAN/GN-3430 |
---|---|---|---|
Compressive Strength | ASTM D-695 | 143(1460) MPa(Kgf/cm | |
Flexural Strength | ASTM D790/ISO 178 | 168(1700) kg/cm²(MPa)[Lb/in²] | |
Flexural Modulus | ASTM D-790 | 7355(75100) MPa(Kgf/cm | |
Tensile Elongation?(Break) | ASTM D638/ISO 527 | 2.5 % | |
Tensile Strength | 121(1230) kg/cm²(MPa)[Lb/in²] | ||
Flexural Strength | ASTM D-790 | 168(1700) MPa(Kgf/cm | |
Charpy impact strength | ASTM D256/ISO 179 | 108(11) kg·cm/cm(J/M)ft·lb/in | |
Tensile Modulus | ASTM D-638 | 8240(84000) MPa(Kgf/cm | |
Dielectric Constant | 10 | ASTM D-150 | 3.41 |
Tensile Modulus | ASTM D638/ISO 527 | 8240(84000) kg/cm²(MPa)[Lb/in²] | |
Tensile Elongation | 断裂 | ASTM D-638 | 2.5 % |
Rockwell Hardness | ASTM D-785 | 93 M标度 | |
Tensile Strength | ASTM D-638 | 121(1230) MPa(Kgf/cm | |
Flexural Modulus | ASTM D790/ISO 178 | 7355(75100) kg/cm²(MPa)[Lb/in²] |
Other | Test Condition | Test Method | TEIJIN JAPAN/GN-3430 |
---|---|---|---|
characteristic | 阻燃型 |
Physical Properties | Test Condition | Test Method | TEIJIN JAPAN/GN-3430 |
---|---|---|---|
Moisture Absorption 23℃/24H | ASTM D570/ISO 62 | 0.12 % | |
Density | ASTM D792/ISO 1183 | 1.44 |
Electrical Properties | Test Condition | Test Method | TEIJIN JAPAN/GN-3430 |
---|---|---|---|
Notched Izod Impact Strength | 艾氏、带缺口厚度6.4mm | ASTM D-256 | 108(11) J/m(kgf·cm/cm) |
Dissipation Factor?(Tangent) | 10 | ASTM D-150 | 0.009 |
Dielectric Constant | 3.51 60Hz | ||
Comparative Tracking Index | IEC 112 | 185 V | |
Insulation failure strength | 快速加压值厚度1.6mm | ASTM D-149 | 30 KV/mm |
Volume Resistivity | ASTM D-257 | 1×10 Ω.cm | |
Dissipation Factor?(Tangent) | 60Hz | ASTM D-150 | 0.0009 |
Arc Resistance | ASTM D-495 | 100 sec | |
Notched Izod Impact Strength | 艾氏、带缺口厚度3.2mm | ASTM D-256 | 108(11) J/m(kgf·cm/cm) |
Processing | Test Condition | Test Method | TEIJIN JAPAN/GN-3430 |
---|---|---|---|
Modeling Shrinkage | 垂直方向 | ASTM D-955 | 0.3~0.5 % |
流动方向 | 0.02~0.2 % |