Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PMMA CMH454 Lucite (Taiwan)
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic performance | Test Condition | Test Method | Lucite (Taiwan)/CMH454 |
---|---|---|---|
melt mass-flow rate | ISO 1133 | 0.8 g/10min | |
density | ISO 1183 | 1.18 g/cm | |
Water absorption rate | Equilibrium,23℃,50% RH | ISO 62 | 0.3 % |
Mechanical properties | Test Condition | Test Method | Lucite (Taiwan)/CMH454 |
---|---|---|---|
Impact strength of cantilever beam gap | ISO 180 | 2.2 KJ/m | |
Tensile stress | 屈服 | ISO 527-2 | 85 MPa |
Impact strength of simply supported beam without notch | ISO 179/1eU | 26 KJ/m | |
Tensile strain | 屈服 | ISO 527-2 | 5 % |
Dart impact | ASTM D3763 | 0.6 J | |
Charpy Notched Impact Strength | ISO 179/1eA | 2.2 KJ/m | |
Flexural modulus | ISO 178 | 3400 MPa | |
bending strength | ISO 178 | 120 MPa |
optical performance | Test Condition | Test Method | Lucite (Taiwan)/CMH454 |
---|---|---|---|
transmittance | ASTM D1003 | 92 % | |
refractive index | ASTM D542 | 1.49 | |
Haze ratio | ASTM D1003 | 0.4 % |
physical property | Test Condition | Test Method | Lucite (Taiwan)/CMH454 |
---|---|---|---|
Rockwell hardness | M-Scale | ISO 2039-2 | 99 |
ball-indentation hardness | ISO 2039-1 | 190 MPa |
Thermal performance | Test Condition | Test Method | Lucite (Taiwan)/CMH454 |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2B | 106 ℃ |
1.8MPa,未退火,HDT | ISO 75-2A | 102 ℃ | |
Linear coefficient of thermal expansion | 流动 | ASTM D696 | 0.000071 cm/cm/℃ |
GWIT | IEC 60695-2-13 | 650 ℃ | |
vicat | ISO 306A | 117 ℃ | |
ISO 306B | 108 ℃ | ||
UL flame retardant rating | UL 94 | HB |