Ethylene Copolymer Escorene™ Ultra LD 705.MJ Molding ExxonMobil
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Test ConditionTest MethodExxonMobil/Escorene™ Ultra LD 705.MJ Molding
tensile strength 断裂ASTM D63815.5 MPa
Shore hardness邵氏A,15秒ASTM D224077
Vinyl acetate contentExxonMobilMethod12.8 wt%
elongation屈服ASTM D638180 %
Flexural modulusASTM D79087.6 MPa
tensile strength 屈服ASTM D6386.31 MPa
elongation断裂ASTM D638>800 %
Dart impact23°CASTM D376319.0 J
-40°CASTM D376332.5 J
melt mass-flow rate190°C/2.16kgASTM D12380.40 g/10min
Shore hardness邵氏D,15秒ASTM D224039
vicatASTM D152577.0 °C