Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP PP1013H1 EXXONMOBIL USA
ExxonMobil™
Automotive sector、chip、Seals、Laboratory equipment、Medical/nursing supplies、Medical packaging
Easy to color、Dimensional stability、High impact
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | EXXONMOBIL USA/PP1013H1 |
---|---|---|---|
Shore hardness | 邵氏D | ISO 868 | 68 |
Mechanical properties | Test Condition | Test Method | EXXONMOBIL USA/PP1013H1 |
---|---|---|---|
Tensile modulus | ISO 527-2/1 | 1570 Mpa | |
tensile strength | 屈服 | ISO 527-2/50 | 34.0 Mpa |
Flexural modulus | ISO 178 | 1350 Mpa | |
Tensile strain | 屈服 | ISO 527-2/50 | 9.3 % |
physical property | Test Condition | Test Method | EXXONMOBIL USA/PP1013H1 |
---|---|---|---|
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 7.5 g/10min |
Thermal performance | Test Condition | Test Method | EXXONMOBIL USA/PP1013H1 |
---|---|---|---|
melting temperature | ISO 11357-3 | 160 °C | |
vicat | ISO 306/A50 | 153 °C | |
Crystallization peak temperature | ISO 11357-3 | 113 °C | |
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 85.7 °C |
1.8MPa,未退火,HDT | ISO 75-2/A | 52.3 °C |