EHMWPE Plaslube® PE 4000 AS Techmer Polymer Modifiers
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Techmer Polymer Modifiers/Plaslube® PE 4000 AS |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C,3.18mm | ASTM D256 | 无断裂 |
hardness | Test Condition | Test Method | Techmer Polymer Modifiers/Plaslube® PE 4000 AS |
---|---|---|---|
Rockwell hardness | R级 | ASTM D785 | 66 |
Mechanical properties | Test Condition | Test Method | Techmer Polymer Modifiers/Plaslube® PE 4000 AS |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 80 % |
tensile strength | ASTM D638 | 32.4 MPa | |
Flexural modulus | ASTM D790 | 896 MPa | |
coefficient of friction | 与钢-动态 | ASTM D1894 | 0.27 |
bending strength | ASTM D790 | 48.3 MPa | |
coefficient of friction | 与钢-静态 | ASTM D1894 | 0.19 |
磨损因数 | ASTM D1894 | 120 10^-8mm³/N·m |
Electrical performance | Test Condition | Test Method | Techmer Polymer Modifiers/Plaslube® PE 4000 AS |
---|---|---|---|
Volume resistivity | ASTM D257 | 1.0E+9到1.0E+11 ohms·cm | |
dielectric strength | ASTM D149 | 20 kV/mm |
physical property | Test Condition | Test Method | Techmer Polymer Modifiers/Plaslube® PE 4000 AS |
---|---|---|---|
Water absorption rate | 24hr | ASTM D570 | 0.070 % |
density | ASTM D792 | 0.969 g/cm³ | |
Shrinkage rate | MD:3.18mm | ASTM D955 | 2.2 % |
Thermal performance | Test Condition | Test Method | Techmer Polymer Modifiers/Plaslube® PE 4000 AS |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 54.4 °C |
0.45MPa,未退火,HDT | ASTM D648 | 93.3 °C | |
Linear coefficient of thermal expansion | MD | ASTM D696 | 9.5E-05 cm/cm/°C |