Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PS Innova N 1921 VIDEOLAR BRAZIL
--
Packaging, household goods
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | VIDEOLAR BRAZIL/Innova N 1921 |
|---|---|---|---|
| Rockwell hardness | M-Sale | ISO 2039-2 | 80 |
| M-Scale | ASTM D785 | 80 |
| thermal performance | Test Condition | Test Method | VIDEOLAR BRAZIL/Innova N 1921 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ASTMD648 | 81.0 °C |
| Vicat softening temperature | -- | ASTMD15254 | 92.0 °C |
| -- | ASTMD15255 | 88.0 °C |
| mechanical properties | Test Condition | Test Method | VIDEOLAR BRAZIL/Innova N 1921 |
|---|---|---|---|
| bending strength | 23°C | ASTM D790 | 75.0 MPa |
| 23°C | ISO 178 | 73.0 MPa | |
| elongation | Break,23°C | ISO 527-2 | 1.4 % |
| Break,23°C | ASTM D638 | 1.7 % | |
| Tensile modulus | 23°C | ASTMD638 | 3200 MPa |
| tensile strength | Break,23°C | ASTM D638 | 44.0 MPa |
| Break,23°C | ISO 527-2 | 43.0 MPa |
| Physical properties | Test Condition | Test Method | VIDEOLAR BRAZIL/Innova N 1921 |
|---|---|---|---|
| density | ASTMD792 | 1.05 g/cm³ | |
| melt mass-flow rate | 200°C/5.0kg | ASTMD1238 | 21 g/10min |
| Shrinkage rate | MD | ASTM D955 | 0.30to0.60 % |
| -- | ISO 294-4 | 0.30to0.60 % | |
| Water absorption rate | Saturation | ASTM D570 | <0.10 % |
| Saturation,23°C | ISO 62 | <0.10 % |
| impact performance | Test Condition | Test Method | VIDEOLAR BRAZIL/Innova N 1921 |
|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 1.8 kJ/m² |
| 23°C,3.20mm | ASTM D256 | 23 J/m |
| flammability | Test Condition | Test Method | VIDEOLAR BRAZIL/Innova N 1921 |
|---|---|---|---|
| UL flame retardant rating | 1.6mm | UL 94 | HB |