| thermal performance | Test Condition | Test Method | DOMO CHEM GERMANY/FL 66G30H1 BK |
|---|---|---|---|
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 255 °C |
| 1.8 MPa, Unannealed | ISO 75-2/A | 245 °C | |
| Melting temperature | ISO 11357-3 | 262 °C | |
| Vicat softening temperature | ISO 306/B50 | 250 °C | |
| Electrical performance | Test Condition | Test Method | DOMO CHEM GERMANY/FL 66G30H1 BK |
| Volume resistivity | IEC 60093 | 1.0E+15 ohms·cm | |
| Surface resistivity | IEC 60093 | 1.0E+13 ohms | |
| mechanical properties | Test Condition | Test Method | DOMO CHEM GERMANY/FL 66G30H1 BK |
| Tensile strain | Break | ISO 527-2/5 | 2.5 % |
| Tensile modulus | ISO 527-2/1 | 8500 Mpa | |
| tensile strength | Break | ISO 527-2/5 | 130 Mpa |
| flammability | Test Condition | Test Method | DOMO CHEM GERMANY/FL 66G30H1 BK |
| ISO | ISO 1874 | PA6.M.14-080.GF30 | |
| UL flame retardant rating | 0.8 mm | UL 94 | HB |
| Burning rate | FMVSS 302 | < 100 mm/min | |
| injection | Test Condition | Test Method | DOMO CHEM GERMANY/FL 66G30H1 BK |
| Mold temperature | 90 to 110 °C | ||
| drying temperature | 75 to 85 °C | ||
| Processing (melt) temperature | 270 to 290 °C | ||
| drying time | 2.0 to 4.0 hr | ||
| impact performance | Test Condition | Test Method | DOMO CHEM GERMANY/FL 66G30H1 BK |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 35 kJ/m² |
| Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 30 kJ/m² |