machinabilityTest ConditionTest MethodMITSUBISHI ENGINEERING JAPAN/GS2030MR2 979G
Dry conditions热风干燥 120℃---約4-8小时
Mold temperature80-120 °C
Processing temperature270-290 °C
Screw speed50-100 rpm
Electrical performanceTest ConditionTest MethodMITSUBISHI ENGINEERING JAPAN/GS2030MR2 979G
Dielectric constantASTM D150/IEC 602503.6
Surface resistivityASTM D257/IEC 600932E+15 Ω
Volume resistivityASTM D257/IEC 600932E+14 Ω.cm
Dielectric lossASTM D150/IEC 602500.0011
mechanical propertiesTest ConditionTest MethodMITSUBISHI ENGINEERING JAPAN/GS2030MR2 979G
Tensile modulusASTM D638/ISO 5278900 kg/cm²(MPa)[Lb/in²]
Elongation at BreakASTM D638/ISO 5272.5 %
Bending modulusASTM D790/ISO 1788500 kg/cm²(MPa)[Lb/in²]
bending strengthASTM D790/ISO 178180 kg/cm²(MPa)[Lb/in²]
Physical propertiesTest ConditionTest MethodMITSUBISHI ENGINEERING JAPAN/GS2030MR2 979G
densityASTM D792/ISO 11831.43