Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Reference Price
| mechanical properties | Test Condition | Test Method | FORMOSA NINGBO/ANC160 |
|---|---|---|---|
| bending strength | D-790 | 671 kg/cm2 | |
| elongation | D-638 | 20 % | |
| tensile strength | D-638 | 399 kg/cm2 | |
| Bending modulus | D-790 | 23000 kg/cm2 | |
| Impact strength of cantilever beam gap | 1/4" | D-256 | 25.8 kg-cm/cm |
| Physical properties | Test Condition | Test Method | FORMOSA NINGBO/ANC160 |
| melt mass-flow rate | 200℃×5KG | D-1238 | 4.4 |
| thermal performance | Test Condition | Test Method | FORMOSA NINGBO/ANC160 |
| Hot deformation temperature | 1/4”,Unannealed | D-790 | 82 °C |
| Flame retardancy | 2.5mm | UL 94 | V-0 |