Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66 GERMAMID 6.6 GF 30 KZH Kunststoff-Kontor-Hamburg GmbH
--
--
Filler, glass fiber reinforced material, 30%, filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Kunststoff-Kontor-Hamburg GmbH/GERMAMID 6.6 GF 30 KZH |
---|---|---|---|
Impact strength of simply supported beam without notch | ISO 179/1eU | 60 kJ/m² | |
Charpy Notched Impact Strength | ISO 179/1eA | 20 kJ/m² |
Mechanical properties | Test Condition | Test Method | Kunststoff-Kontor-Hamburg GmbH/GERMAMID 6.6 GF 30 KZH |
---|---|---|---|
Tensile modulus | ISO 527-2 | 9000 MPa | |
Tensile strain | 断裂 | ISO 527-2 | 3.5 % |
tensile strength | 屈服 | ISO 527-2 | 140 MPa |
Electrical performance | Test Condition | Test Method | Kunststoff-Kontor-Hamburg GmbH/GERMAMID 6.6 GF 30 KZH |
---|---|---|---|
Surface Resistivity | IEC 60093 | 1E+13 ohms |
physical property | Test Condition | Test Method | Kunststoff-Kontor-Hamburg GmbH/GERMAMID 6.6 GF 30 KZH |
---|---|---|---|
Shrinkage rate | ISO 294-4 | 0.30to1.0 % | |
Water absorption rate | 饱和,23°C | ISO 62 | 1.5 % |
density | ISO 1183 | 1.32 g/cm³ |
Thermal performance | Test Condition | Test Method | Kunststoff-Kontor-Hamburg GmbH/GERMAMID 6.6 GF 30 KZH |
---|---|---|---|
thermal conductivity | ISO 8302 | 0.24 W/m/K | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 240 °C |
melting temperature | 255 °C |