Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PLA EcoVid 43TF Greener Polymers Inc.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | Greener Polymers Inc./EcoVid 43TF |
|---|---|---|---|
| Crystallization peak temperature | DSC | ASTM D3418 | 155to170 °C |
| Glass transition temperature | ASTM D3418 | 55.0to60.0 °C | |
| Hot deformation temperature | HDT | ASTME2092 | 80to110 °C |
| Melting temperature | ASTM D3418 | 130to180 °C | |
| Vicat softening temperature | ASTM D1525 | 130 °C |
| mechanical properties | Test Condition | Test Method | Greener Polymers Inc./EcoVid 43TF |
|---|---|---|---|
| bending strength | ASTM D790 | 108 MPa | |
| elongation | Break | ASTM D638 | 3.5 % |
| tensile strength | Yield | ASTM D638 | 62.1 MPa |
| Physical properties | Test Condition | Test Method | Greener Polymers Inc./EcoVid 43TF |
|---|---|---|---|
| density | ASTM D792 | 1.27 g/cm³ | |
| melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 6.0 g/10min |
| RelativeViscosity | ASTM D1238 | 2.5 | |
| 210°C/2.16kg | ASTM D1238 | 6.0 g/10min | |
| 收缩率-Flow | ASTM D1238 | 0.30to0.50 % |
| impact performance | Test Condition | Test Method | Greener Polymers Inc./EcoVid 43TF |
|---|---|---|---|
| Impact strength of cantilever beam gap | ASTM D256 | 16 J/m |
| optical performance | Test Condition | Test Method | Greener Polymers Inc./EcoVid 43TF |
|---|---|---|---|
| Clarity | NIL |