Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC 7022FD2 MITSUBISHI ENGINEERING JAPAN
IUPILON™
Medical packaging
Low viscosity,transparent
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
machinability | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/7022FD2 |
---|---|---|---|
Dry conditions | 热风干燥 120℃---约4-8小时 | ||
Mold temperature | 70-100 °C | ||
Processing temperature | 260-280 °C | ||
Screw speed | 50-100 rpm |
mechanical properties | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/7022FD2 |
---|---|---|---|
Bending modulus | ASTM D790/ISO 178 | 2100 kg/cm²(MPa)[Lb/in²] | |
bending strength | ASTM D790/ISO 178 | 90 kg/cm²(MPa)[Lb/in²] | |
Elongation at Break | ASTM D638/ISO 527 | 124 % | |
Tensile modulus | ASTM D638/ISO 527 | 2500 kg/cm²(MPa)[Lb/in²] |
Electrical performance | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/7022FD2 |
---|---|---|---|
Surface resistivity | ASTM D257/IEC 60093 | 6E+15 Ω | |
Volume resistivity | ASTM D257/IEC 60093 | 3E+14 Ω.cm |
Physical properties | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/7022FD2 |
---|---|---|---|
density | ASTM D792/ISO 1183 | 1.21 | |
Shrinkage rate | ASTM D955 | 0.5 - 0.7 % |